3mancannon
New member
- Joined
- Sep 19, 2025
- Messages
- 2
I'm still learning TIG welding and working on old car parts. Lately I've been fixing cast intake manifolds that are worn out from heat and dirt.
Here's what I'm using:
-180 amps with 350°F preheat
-3/32" tungsten
-#7 gas lens20 cfh argon
-60% AC balance, 50Hz
-Cleaned with acetone, stainless brush, and burr
-4043 filler rod
The weld looks good at first, but after it cools, I see small cracks near the edges. I think it might be from how the part cools or maybe dirt inside the metal. Has anyone had this happen with old cast stuff? What helped you fix it?
Here's what I'm using:
-180 amps with 350°F preheat
-3/32" tungsten
-#7 gas lens20 cfh argon
-60% AC balance, 50Hz
-Cleaned with acetone, stainless brush, and burr
-4043 filler rod
The weld looks good at first, but after it cools, I see small cracks near the edges. I think it might be from how the part cools or maybe dirt inside the metal. Has anyone had this happen with old cast stuff? What helped you fix it?